Deterioration in the Mechanical Strength of Commercial Carbon Steels Exposed in Various Environments
Memoirs of the Faculty of Engineering, Yamaguchi University Volume 31 Issue 1
Page 61-70
published_at 1980
Title
実用炭素鋼板材の環境中における強度低下について
Deterioration in the Mechanical Strength of Commercial Carbon Steels Exposed in Various Environments
Creators
Takimoto Akio
Creators
Tanaka Hiroshi
Creators
Kazusa Nobuhiro
Creators
Fukuhara Hiroyuki
Creators
Sasaki Toyoshi
Source Identifiers
It is the purpose of this study to investigate losses in the tensile strength ratio, the true fracture strain ratio and the absorbed energy ratio to fracture of three different commercial carbon steels exposed in various environments of the air, the sea, the river and the soil. The results are given as parabolic functions of elapsed time in each environment. The concentration of the SO_2 content in the air was sensitive to the absorbed energy ratio of the SS-41 steel plate of one millimeter thickness in bright finished condition. Scale products yielded on three different steel specimens exposed in the air were examined by the X-ray diffraction method. Majority of them were determined to be the iron hydroxide FeO (OH) and no traces of iron oxides such as FeO, Fe_3O_4 and Fe_2O_3,iron sulfates such as FeSO_4 and iron chlorides such as FeCl_2 were confirmed.
Languages
jpn
Resource Type
departmental bulletin paper
Publishers
山口大学工学部
Date Issued
1980
File Version
Version of Record
Access Rights
open access
Relations
[ISSN]0372-7661
[NCID]AN00244228
Schools
工学部