The Chemical Durability of SiO_2-B_2O_3-Na_2O System Glasses
        Memoirs of the Faculty of Engineering, Yamaguchi University Volume 22 Issue 1
        Page 121-129
        
    published_at 1971
            Title
        
        SiO_2-B_2O_3-Na_2O系ガラスの化学的耐久性
        The Chemical Durability of SiO_2-B_2O_3-Na_2O System Glasses
        
    
                
                    Creators
                
                    Yatabe Shunichi
                
                
            
            
                
                    Creators
                
                    Date Yasuhumi
                
                
            
            
                
                    Creators
                
                    Harada Yoshio
                
                
            
    
        
            Source Identifiers
        
    
    
            Creator Keywords
        
            Bridge Management System (BMS)
            maintenance
            repair
            strengthening
            bridge rating
            life cycle cost
            inspection
    The chemical durability of SiO_2-B_2O_3-Na_2O system glasses was studied in this paper. The thirty kinds of glasses in this system were fused in the electric furnace. The fused glasses were powdered into the particles of 35-60 meshes (Tyler), and 2g of them were immersed in 50ml water of 30,50 and 70℃, while being stirred during 10,20,40 and 80 minutes respectively. Then the amounts of alkali dissolved into the water were measured by 0.01N HCl. The results were as follows. (1) The experimental data were tested by analysis of variance, and it was found that log of dissolved amounts was linear function of log of dissolving time, and was linear function of reciprocal of absolute temperature of the water. (2) In the case of Na_2O mol constant, the dissolving phenomena were very simple. That is, the dissolved amounts increased considerably with increasing B_2O_3/SiO_2. (3) In the case of SiO_2 mol constant, the dissolving phenomena were very complex. Namely, there were maximum and minimum value of dissolved amounts. (4) Generally, the glasses in the outer domain of exsolution were more durable than the glasses in the inner domain.
        
        
            Languages
        
            jpn
    
    
        
            Resource Type
        
        departmental bulletin paper
    
    
        
            Publishers
        
            山口大学工学部
    
    
        
            Date Issued
        
        1971
    
    
        
            File Version
        
        Version of Record
    
    
        
            Access Rights
        
        open access
    
    
            Relations
        
            
                
                
                [ISSN]0372-7661
            
            
                
                
                [NCID]AN00244228
            
    
        
            Schools
        
            工学部
    
                