Contents Menu

The Chemical Durability of V_2O_5-P_2O_5 System and V_2O_5-P_2O_5-BaO System Glasses (Continued Report)

Memoirs of the Faculty of Engineering, Yamaguchi University Volume 21 Issue 1 Page 23-33
published_at 1970
KJ00002585410.pdf
[fulltext] 758 KB
Title
V_2O_5-P_2O_5系およびV_2O_5-P_2O_5-BaO系ガラスの化学的耐久性(続報)
The Chemical Durability of V_2O_5-P_2O_5 System and V_2O_5-P_2O_5-BaO System Glasses (Continued Report)
Creators Yatabe Shunichi
Creators Okada Toshio
Creators Sugimoto Kojin
Creators Mori Masami
Source Identifiers
Creator Keywords
RF-MBE GaN localized exciton photoluminescence temperature dependence
This report is a further study on the previous report. In the previous report, it was assumed that the dissolving phenomena of various ions in glasses into the water followed Moriya's theoretical equation, and the data was examined quantitatively. In this report, it is assumed that the dissolving phenmena follow Douglas' equation, and they are tested by analysis variance. The conclusions are as follows. 1) The dissolving phenomena of P conform accurately to the theoretical equation, that is, log of the dissolving amounts of P vary linearly with log of the dissolving time and they are linear function of reciprocal of absolute temperature. 2) The dissolving phenomena of V and Ba are not in accordance with the theoretical equation as a whole, but they obey approximately the equation in some case, and in several case they obey exactly the equation. 3) Log of concentration of H ion in aqueous solution containing various ions dissolved from glasses varies linearly with log of stirring time and reciprocal of absolute temperature in the case of VO_<2.5> 40 mol. 4) Generally theoretical equations give the exact description of dissolving phenomena in the case of VO_<2.5> 40mol.
Subjects
材料工学 ( Other)
Languages jpn
Resource Type departmental bulletin paper
Publishers 山口大学工学部
Date Issued 1970
File Version Version of Record
Access Rights open access
Relations
[ISSN]0372-7661
[NCID]AN00244228
Schools 工学部